Focuses On Professional Cleanroom Project And Pharmaceutical Cleanroom Equipment.
The punch is cracked and missing corners, metal shavings may be embedded in the tablet. Due to improper heat treatment of the punch, its own damage and cracks have not been carefully inspected, cannot withstand the pressure or the pressure of the tablet press is too high, and may cause bursting when inhibiting the crystallized drug. The heat treatment method of the punch should be improved, the quality of the punch should be enhanced, the pressure should be adjusted, and the appearance of the tablet should be checked. If you notice a break, you should immediately spot the chip and find a reason to overcome it. The punch is broken or the neck of the tail is broken. Due to improper heat treatment of the mold, the mold itself was not carefully inspected for damage and